Unconfined Compression Test
The samples' length to diameter ratio (L/D) must be between and, according to ASTM (American Society for Testing and Materials) and according to ISRM (International Society for Rock Mechanics). The cylindrical surfaces are prepared in order to be flat and smooth. In particular, the sample's ends must be leveled within a millimeters tolerance and they .